That "crack" can be what's called a "fold" in the surface of the casting. If the material is thick enough it is only cosmetically annoying. It -can- be a stress riser if it goes more than a third of the way in. Happens as the molten iron contacts the mold, cools more at the contact surface and "drags". If that were a part to be machined it would be different. As it is, if dye penetrant or Magnaflux tested and found to be surface only, don't fret.